Figure 4: Flexural strength of the control group and plasma-treated polypropylene fiber-reinforced test group by varying fiber Wt% and fiber length. (a) Flexural strength of the plasma treated polypropylene fiber-reinforced polymethyl methacrylate at 2.5. (b) Flexural strength of the plasma-treated polypropylene fiber-reinforced polymethyl methacrylate at 5 Wt%. (c) Flexural strength of the plasma-treated polypropylene fiber-reinforced polymethyl methacrylate at 10 Wt%. (d) Flexural strength of the 3mm long plasma-treated polypropylene fiber-reinforced polymethyl methacrylate. (e) Flexural strength of the 6mm long plasma treated polypropylene fiber-reinforced polymethyl methacrylate. (f) Flexural strength of the 12mm long plasma-treated polypropylene fiber-reinforced polymethyl methacrylate

Figure 4: Flexural strength of the control group and plasma-treated polypropylene fiber-reinforced test group by varying fiber Wt% and fiber length. (a) Flexural strength of the plasma treated polypropylene fiber-reinforced polymethyl methacrylate at 2.5. (b) Flexural strength of the plasma-treated polypropylene fiber-reinforced polymethyl methacrylate at 5 Wt%. (c) Flexural strength of the plasma-treated polypropylene fiber-reinforced polymethyl methacrylate at 10 Wt%. (d) Flexural strength of the 3mm long plasma-treated polypropylene fiber-reinforced polymethyl methacrylate. (e) Flexural strength of the 6mm long plasma treated polypropylene fiber-reinforced polymethyl methacrylate. (f) Flexural strength of the 12mm long plasma-treated polypropylene fiber-reinforced polymethyl methacrylate